Phosphoric acid meets the grating resin through dilute to mid-strength splash and wetting. The reference chart lists phosphoric below 50 % and below 40 °C as C for ortho, B for iso, A for vinyl ester and epoxy. The rating still depends on concentration and temperature; high concentration or hot contact should be reviewed before specification.
- Listed basis: phosphoric <50 % <40 °C — ortho C, iso B, VE A, epoxy A.
- Process and washdown exposure varies in strength; the listed grade follows the actual band.
- Concentrated or hot phosphoric service goes to engineering compatibility review.
1. Process liquor and washdown contact
Phosphoric reaches the resin face in process splash, channel wetting and washdown around treatment and production areas. At the listed band, VE and epoxy hold an A reading, iso a more conservative B, and ortho a C that should not be selected for this acid contact. Fibres stay protected behind whichever matrix keeps the face sealed.
Residue from phosphoric service can dry on the panel and concentrate the acid locally. Cut edges and worn grit give that residue a path toward the reinforcement, so finish condition and edge seal are checked alongside the resin family rather than assumed adequate.
| Process stage | Ortho | Iso | VE | Epoxy |
|---|---|---|---|---|
| Phosphoric <50 %, <40 °C | C | B | A | A |
2. Matching the resin to the strongest stage
The chart row covers phosphoric under 50 % and under 40 °C. Iso B is a splash and intermittent-wetting reading, while VE and epoxy A describe the stronger face at this band. A higher strength, hotter wash or continuous immersion moves the grade down and calls for a fresh compatibility check rather than carrying the listed reading forward.
Service can differ between process liquor and washdown water, and strength may shift between stages. The resin should be matched to the strongest and hottest condition the panel meets, not an average or nominal value; an acidic condensate or residue stream also needs its own composition review.
3. Selections that carry a milder assumption
Assuming phosphoric stays mild across every concentration and extending an iso B to concentrated or hot service misses the duty: above the listed band the grade drops, and the panel needs review rather than the conservative reading carried over. Selecting ortho for this acid is another miss; ortho reads C and is not rated for the contact.
A washdown panel left soaking in phosphoric liquor should not inherit an intermittent-wetting rating; immersion is a stricter mode needing its own basis. Mixed acidic effluent also cannot be resolved from the phosphoric row alone, and any residue that concentrates on the face should be assessed for its local load.
| Phosphoric case | Risk | Confirmation needed |
|---|---|---|
| Ortho in phosphoric service | Matrix reads C; unrated | Iso, VE or epoxy per basis |
| Concentrated or hot liquor | Grade drops above band | Written compatibility review |
| Continuous soaking | Soaking outside splash basis | Separate immersion confirmation |
| Mixed acidic effluent | Component rating does not cover blend | Full-liquor evaluation on data |
4. Site inspection and the order record
On phosphoric walkways, note liquor strength, panel temperature and dried residue; look for dulling, softened patches or lifted edges, and inspect bar skin, clip fit and cut seals each pass against the service notes.
Order details to supply: the phosphoric strength range, temperature range and how the acid touches the panel. The concentration and temperature bounds for the grade, plus any concentrated or hot exposure, must be confirmed through the factory or engineering review before the unit carries duty.
5. Frequently Asked Questions
Which resin suits phosphoric acid exposure on FRP grating?
The family is set by phosphoric acid, concentration, heat and contact type. The reference chart lists this medium within its stated envelope; those ratings apply only to the stated conditions. Phosphoric service still depends on concentration and temperature; high concentration or hot contact should be reviewed before specification.
Is phosphoric acid covered by the reference compatibility chart?
Yes, within the listed concentration and temperature envelope. Anything outside the listed conditions moves the grade down and needs a documented review rather than a table read.
Does this resin choice certify food-safe or drinking-water use?
No. Food-contact and drinking-water compliance are not established from the resistance chart. Where the project requires such approval, obtain the matched compliance document and verify it against the destination regulation before ordering.
What changes the resistance rating besides the resin family?
Concentration, heat and contact type all move the rating. At higher temperature or concentration the grade drops one step; immersion is stricter than splash or intermittent wetting.
What must be confirmed before an order for this service?
Provide the exact medium, min/max concentration, min/max temperature and contact type. Critical, hot, concentrated or unlisted exposure needs a written factory confirmation or project-specific test; combined duty stays on technical review.
Keep that record with the inquiry and update it whenever the acid strength, temperature or washing routine changes. A revised record gives the factory a clear basis for review and prevents a later process change from inheriting the old approval.
Reference PDFs: chemical-resistance-table.pdf · resin-selection-guide.pdf