Specify the build-up to the bearer span, match the resin to the KOH concentration, temperature and exposure mode, choose a wet-zone finish, isolate fixings from steel, and close the RFQ with pooling detail and matched documentation; suitability for the recorded conditions is confirmed by project review.
- Caustic strength sets the resin line: polyester tolerates only dilute alkali here, so vinyl ester or epoxy are the families to review for stronger KOH, warmth, mist or pooled wetting.
- Pultruded I-bar follows longer plinth and pipe runs; molded 38 mm panels follow drums, valves and sump openings. Directional strength.
- Grip for operator pads where feet stay damp; concave dished sections shed runoff on splash ledges, and smooth mesh is avoided on the alkali splash line. Unsealed cuts let liquor reach the glass, so site-cut panels are diamond-sawn and edge-sealed before exposure.
How this article differs: This page covers the strong-alkali duty and procurement inputs; it does not re-derive load tables, concentrated-load checks or resin chemistry, which are handled in the dedicated reference articles.
1. Site Conditions and Duty
Potassium hydroxide solution feeds saponification, biochemistry, cleaning-product manufacture and some surface-treatment lines. Grating at the reactor plinth, drum offload and sump cover takes caustic splash when couplings break, drips from pump glands, and runoff that crosses the wet floor before reaching the drain. The atmosphere can carry alkali mist, especially where liquor is agitated or warmed, and residue left after rinsing may concentrate on the bar faces.
Strong alkali attacks certain resin families through saponification and matrix swelling, so the resin choice cannot follow a general moisture label. A polyester that tolerates dilute alkali may not hold up to a stronger KOH liquor; tougher vinyl ester or epoxy families are considered once the recorded concentration, temperature and exposure are reviewed against the resistance tables. Glass fibres are usually protected while the binder stays intact, but an opened or unsealed edge lets alkali reach the reinforcement and undercut the laminate from the cut side.
2. Build-up, Resin and Surface Selection
| Location | Exposure mode | Duty | Suggested build-up | Resin / surface note |
|---|---|---|---|---|
| Reactor plinth | Caustic splash, gland drips, mist | Rounds around vessel and pumps | Pultruded 38 mm I-bar | Resin per recorded alkali; grit top |
| Drum offload apron | Intermittent splash, runoff | Changeover and coupling | Molded 38 mm 38×38 | Matched resin; concave at splash |
| Sump / trench cover | Continuous damp, pooled rinse | Cover over liquid channel | Pultruded 38 mm T-bar | Sealed edge; concave shed |
| Sample valve ledge | Light splash and vapour | Standing inspection reach | Molded 38 mm 50×50 | Grip finish on wet footing |
- Caustic strength sets the resin line: polyester tolerates only dilute alkali here, so vinyl ester or epoxy are the families to review for stronger KOH, warmth, mist or pooled wetting.
- Pultruded I-bar follows longer plinth and pipe runs; molded 38 mm panels follow drums, valves and sump openings. Directional strength.
- Grip for operator pads where feet stay damp; concave dished sections shed runoff on splash ledges, and smooth mesh is avoided on the alkali splash line. Unsealed cuts let liquor reach the glass, so site-cut panels are diamond-sawn and edge-sealed before exposure.
3. Installation and Bearing Details
- Survey the plinth bearers for level, scale and bearing width before dry-fitting; an uneven frame transfers stress onto panel edges in the caustic wet zone.
- Bed sections on the 3 mm neoprene isolation strip over steel, retaining end and side gaps from the node detail around reactors and valves.
- Secure each bar at every bearer and corner with the matching A2-70 M6/M8 clip family; isolate the fixing from dissimilar metal and hand-tighten to setting without over-driving.
- Seal cut edges and drilled holes with matched resin within 24 hours; lift removable covers without prising neighbours, then re-check bearing and clips after the first two weeks.
- ≥ 50 mm bearing on steel/FRP support; 60 mm preferred at end spans
- 3 mm neoprene strip on steel supports to cut galvanic contact and local stress
- 10–15 mm end gap for thermal movement (~20 mm at long runs)
- 6–10 mm side gap for expansion and safe lifting
- Clips at every support and every corner; C/L/T/W/saddle families; A2-70 M6/M8 bolts
- Hand-tighten plus 1/4 turn; do not over-torque
- Seal any cut edge with matched resin within 24 hours
- Walk the deck and re-torque after 2 weeks of service
4. Routine Inspection and Maintenance
| Task | Frequency | What to check |
|---|---|---|
| Visual inspection | Monthly | Cracked bars, loose clips, edge seal, displaced panels |
| Clip torque check | Quarterly, first year | Hand-tight; re-torque any loose fixing |
| Washdown | As needed | Fresh water, low pressure; no acid or solvent-based cleaner |
| Grit top renewal | As needed | Top up worn traction with matched gritted resin |
| Edge seal check | Annually | Touch up any bare roving before it spreads |
| UV top-coat | Every 3–5 years | Re-coat exposed surface with matched resin on request |
- Walk the plinth and apron monthly for softened bars, blistering, loose clips, shifted covers and alkali film in damp corners.
- Check clip torque quarterly in year one; free any seized coupling or gland fitting before it locks under caustic residue.
- Wash down with fresh water at low pressure; keep reciprocal alkali cleaners and solvents off the resin matrix.
- Renew worn grit with matched gritted resin and touch up exposed roving at edge seals before undercutting spreads along the sump.
5. RFQ Inputs and Procurement Checklist
- State the KOH concentration range and recorded operating or ambient temperature so resin can be graded against the resistance table.
- Give the duty: operator rounds, drum changeover, tray carry or equipment reach, and any local load from tools or barrels.
- Mark finishes by zone: grit on wet pads, concave on splash ledges, smooth on dry points.
- Describe drainage and pooling: splash only, runoff to channel, or pooled caustic in a sump, plus contact duration per shift.
- Cite the governing standard and deflection limit; request the matched deflection report, batch material record and Barcol check with the production papers.
- Governing access standard and project deflection limit are cited with the order.
- Matched resistance note confirms the resin grade against the recorded medium.
- Batch material record and Barcol hardness check accompany the delivered panels.
- Any point, wheel, concentrated or equipment load is referred to engineer review and the matched report.
| Minimum order (MOQ) | 10 m² |
| Standard production | 15–25 working days after drawing approval |
| Overall lead time | 12–36 working days overall |
| Indicative price | USD 15–95/m² |
| Manufacturing history | Founded 2004; 200+ employees; 20,000+ m² plant |
| Export reach | 45+ countries; 541+ customer reviews, 4.9/5 average rating |
6. Compliance and Service Boundaries
7. Frequently Asked Questions
Which resin resists potassium hydroxide on grating?
The grade follows the recorded concentration, temperature and contact type. Ordinary polyester is a mild-alkali baseline; vinyl ester or epoxy are considered for stronger KOH, warmth, mist or pooled wetting after checking the resistance reference. Suitability remains a project evaluation, not a blanket claim.
Pultruded or molded around a caustic reactor?
Pultruded I-bar carries longer plinth and pipe runs with less weight; molded 38 mm sections shape cleanly around drums, valves and sump openings. The measured span and fittings decide the mix.
How should a wet caustic floor be finished?
Grit-embedded top for pads where feet stay damp; concave dished sections shed runoff on splash ledges; keep smooth panels away from the alkali line. Match the opening to site footwear.
How are panels isolated from steel supports?
Sections bed on the 3 mm neoprene strip, and matching clips fasten bars to bearers and corners with the fastener isolated from dissimilar metal. End and side gaps follow the node drawing; bolts are hand-tightened to setting.
What caustic damage signals require review?
Softened or blistered skin, darkening, lifted roving, cracked edge seal or alkali film under clips should be flagged for engineering review; do not paint over or patch a laminate that has opened to the glass.