Span long bar sections across the tower beams, grade the matrix to the scrubbed gas, seal both faces of hatch cuts, keep ventilation gaps open, and send the tower plan and resistance basis with the RFQ.
- Scrubber matrix: vinyl ester suits acid gas, caustic scrub and persistent humid air around the tower; epoxy follows only for a notably aggressive or hotter stream after the resistance review. A general moist-air grade is avoided where gas concentrates at the eliminator or outlet.
- Long-span depth: pultruded I-bar or T-bar carries the wide tower wrap and duct crossing; molded 38 mm fills the recirculation crossing and hatch cut-outs. The vessel width and beam spacing decide whether 38 mm depth clears the deflection limit.
- Duct finish: grit-embedded top at the sampling and fan-standing pads; concave dished members along the damp tower wrap; smooth mesh reserved for sheltered duct stretches clear of drift.
How this article differs: This page covers scrubber and duct access selection; it does not size the packing bed, fan or exhaust stack, or detail resin chemistry, which remain in the dedicated references.
1. Site Conditions and Duty
Wet scrubbers and their exhaust ducts treat acid or alkaline off-gas before discharge; a service platform wraps the tower and crosses to the ductwork so operators can reach mist eliminators, recirculation pumps and sampling ports. Gas drift around the vessel, condensate from cooler duct walls and persistent humid air keep the deck damp, and an unsealed edge over the tower stays exposed to that moist film. Steel members at the duct support pit in such air, while composite decking holds its section and stays light across the wide tower-to-duct spans.
The route combines a tower walk around the vessel, a duct-side platform at the fan outlet and stack connection, and a crossing over the recirculation line. Long spans between support beams govern the deck depth; ductwork, fans and dampers hang from their own structure rather than the grating. Condensate runs off the lower bar, and the opening must stay open for gas movement around the tower instead of being capped by a solid finish.
Exposure mixes the scrubbed gas type with recurring dampness, so the matrix follows the more aggressive stream rather than the humidity alone. Where a caustic or acid recirculation liquor drips onto the platform, that local patch needs a grade matched to the liquor; sheltered duct stretches away from the vessel see lighter contact and can take a calmer finish.
2. Build-up, Resin and Surface Selection
| Scrubber zone | Gas / moisture | Service | Section | Matrix / duct note |
|---|---|---|---|---|
| Tower wrap walk | Acid or alkaline gas, condensate | Reach eliminator, sample port | Pultruded 38 mm I-bar | Vinyl ester; concave |
| Duct-side platform | Gas drift, humid air | Fan outlet, stack connection | Pultruded 38 mm T-bar | Resin per recorded gas |
| Recirculation line crossing | Liquor drips, damp cycling | Cross over pump line | Molded 38 mm 38×38 | VE matrix; grit top |
| Tower service hatch | Intermittent lift-out | Removable over vessel | Molded 38 mm cut-to-size | Resin-sealed cut ends |
- Scrubber matrix: vinyl ester suits acid gas, caustic scrub and persistent humid air around the tower; epoxy follows only for a notably aggressive or hotter stream after the resistance review. A general moist-air grade is avoided where gas concentrates at the eliminator or outlet.
- Long-span depth: pultruded I-bar or T-bar carries the wide tower wrap and duct crossing; molded 38 mm fills the recirculation crossing and hatch cut-outs. The vessel width and beam spacing decide whether 38 mm depth clears the deflection limit.
- Duct finish: grit-embedded top at the sampling and fan-standing pads; concave dished members along the damp tower wrap; smooth mesh reserved for sheltered duct stretches clear of drift.
- Worked example: a pultruded 38 mm I-bar over a 1200 mm single clear span, checked to L/200, gives about 9 kN/m² for distributed walking only. This intermittent-access figure omits point contact, hatch lifting force and hung duct weight; the matched report confirms the final beam spacing, and the duct support carries the line.
- Condensate edge: inspect panel undersides and cut-end seals for film buildup, softening or exposed fibre; an edge that lets moist gas wick into the bar degrades over several seasons.
3. Installation and Bearing Details
- Check tower beams and duct supports for straightness, level and corrosion film before dry-fitting; a tilted support passes its unevenness onto bar ends.
- Rest sections on the isolation bedding over steel, keeping node end and side clearances around the tower vessel, duct flanges and hatch frames.
- Anchor each support and corner with the stainless clip suited to the bar; snug by hand to the fitting setting, leaving hatch panels free to lift.
- Close sawn edges and drilled holes on both faces of the cut-out with matched resin; after a wet spell, verify condensate drains and no film has sealed the mesh.
- ≥ 50 mm bearing on steel/FRP support; 60 mm preferred at end spans
- 3 mm neoprene strip on steel supports to cut galvanic contact and local stress
- 10–15 mm end gap for thermal movement (~20 mm at long runs)
- 6–10 mm side gap for expansion and safe lifting
- Clips at every support and every corner; C/L/T/W/saddle families; A2-70 M6/M8 bolts
- Hand-tighten plus 1/4 turn; do not over-torque
- Seal any cut edge with matched resin within 24 hours
- Walk the deck and re-torque after 2 weeks of service
4. Routine Inspection and Maintenance
| Task | Frequency | What to check |
|---|---|---|
| Visual inspection | Monthly | Cracked bars, loose clips, edge seal, displaced panels |
| Clip torque check | Quarterly, first year | Hand-tight; re-torque any loose fixing |
| Washdown | As needed | Fresh water, low pressure; no acid or solvent-based cleaner |
| Grit top renewal | As needed | Top up worn traction with matched gritted resin |
| Edge seal check | Annually | Touch up any bare roving before it spreads |
| UV top-coat | Every 3–5 years | Re-coat exposed surface with matched resin on request |
- Walk the tower wrap checking underside film, cut-end seal condition, loose fixings and hatch panels that bind on the rim.
- Look for softening or exposed fibre near the outlet and eliminator where gas drift concentrates; mark any swollen bar for matrix review.
- Rinse film and residue through the mesh with clean water at low pressure; keep acid or solvent wash off the composite face.
- Renew worn grit at sampling pads and bare fibre at hatch seals; log panels where moisture has reached the roving for edge or section renewal.
5. RFQ Inputs and Procurement Checklist
- Describe the scrubber: gas type, treatment stage, outlet and fan position, and any recorded concentration or temperature.
- Give tower circumference and platform length, beam spacing, hatch and sampling-port sizes, and the access pattern: rounds, eliminator visits or occasional carry.
- Mark outlet pads, damp tower stretches and sheltered duct runs with the finish wanted in each.
- Attach the tower plan showing vessel, hatches, dampers, sampling ports, duct plenum and ventilation gaps.
- Reference the governing standard and deflection limit; request the matched resistance note, deflection report, batch record and hardness check.
- Governing access standard and project deflection limit are cited with the order.
- Matched resistance note confirms the resin grade against the recorded medium.
- Batch material record and Barcol hardness check accompany the delivered panels.
- Any point, wheel, concentrated or equipment load is referred to engineer review and the matched report.
| Minimum order (MOQ) | 10 m² |
| Standard production | 15–25 working days after drawing approval |
| Overall lead time | 12–36 working days overall |
| Indicative price | USD 15–95/m² |
| Manufacturing history | Founded 2004; 200+ employees; 20,000+ m² plant |
| Export reach | 45+ countries; 541+ customer reviews, 4.9/5 average rating |
6. Compliance and Service Boundaries
7. Frequently Asked Questions
What grating spans a scrubber tower and duct?
Pultruded I-bar or T-bar carries the wide tower wrap and duct crossing; molded 38 mm fills recirculation crossings and hatches. Vessel width and beam spacing set the depth against the deflection limit.
Which matrix handles corrosive scrubbed gas?
Vinyl ester suits acid gas, caustic scrub and humid air; epoxy follows for a more aggressive or hotter stream after review. The gas record, concentration and temperature set the grade.
How does condensate damage a tower panel?
Moist film sits on the lower bar and unsealed edge; an open mesh lets it drain, while a solid finish traps it and leads to softening or fibre exposure over time.
Does the platform carry the duct or fan?
No. Ductwork, fans and dampers are held by their own structure; the grating is the walking and cover surface only. Equipment loads need project engineering.
How often is a scrubber platform inspected?
Rounds track underside film, seal ends, fixings and hatch seating; outlet-pad drift and matrix condition are logged, with roving-reached panels going to renewal review.