Grade the vinyl-ester matrix to the recorded alkali, lay a coarse draining mesh around dissolvers and tanks, flush crystalline residue, seal plinth edges, and confirm tank or trolley use through factory review.
- Alkali grade: vinyl ester handles strong caustic and concentrated hydroxide splash; isophthalic polyester may cover a mild dilute alkaline rinse after the resistance record is reviewed, and epoxy is held for a notably aggressive or hotter solution. A general matrix is not specified where concentrated alkali pools at a stand.
- Depth and family: molded 38 mm fills the mixer stand and vessel walk cut around equipment; pultruded I-bar follows the floor runs. The coarser 50×50 opening sheds hydroxide and powder faster; span and walking duty set the depth.
- Film finish: grit-embedded top at the hose standing spots; concave dished members along the recovery trench shed damp film; smooth mesh kept for sheltered corners clear of drips.
How this article differs: This page covers caustic solution platform selection; it does not size the dissolver or tanks, design the containment sump, or detail resin chemistry, which remain in the dedicated references.
1. Site Conditions and Duty
Caustic and alkali solution plants prepare, dilute and feed sodium hydroxide, soda ash or comparable alkaline products around mixing vessels, makeup bins and transfer lines. The walkway and floor catch hydroxide splash at unions, drips from elbows and valves, and a damp film carried by warm solution vapour. Unsuitable matrix under alkali shows swelling, dull efflorescence or a crazed face rather than sharp rust; dried crystals at an edge hold concentrated hydroxide against the bar through repeated drying cycles. Steel uprights pit in the same humid alkaline air, whereas composite members hold their section and avoid the dissimilar-metal contact.
The area centers on the mixer and makeup stand where staff connect hoses, the vessel-side walk around tanks and pumps, and the trench that carries release to the alkali recovery sump. Bar depth follows the walking and light carry duty; the resin matches the strongest alkali and its recorded concentration and temperature. Caustic strength decides the grade: a mild washdown and a concentrated hot hydroxide stream are not interchangeable, and the platform record should name the product instead of a broad alkali label.
Alkali film dries to a powdery residue, so open drainage counts beside chemical tolerance: liquid should run off to the recovery trench rather than rest on a bar, and rinsed-off powder should not pack into the openings. Sawn edges around vessel plinths and hatch cut-outs wick concentrated solution, which makes sealing there as important as it is beside an acid line.
2. Build-up, Resin and Surface Selection
| Makeup mixer stand | Hydroxide splash, warm vapour | Connect hose, sample mix | Molded 38 mm 50×50 | Vinyl ester; grit finish |
|---|---|---|---|---|
| Vessel-side walk | Alkali drips, damp film | Pass tanks and pumps | Pultruded 38 mm I-bar | VE matrix; concave |
| Recovery trench | Powdery residue, rinse water | Route release to alkali sump | Molded 38 mm 38×38 | Resin per recorded alkali |
| Plinth service hatch | Intermittent opening | Lift-out over pump | Molded 38 mm cut-to-size | Resin-sealed edges |
- Alkali grade: vinyl ester handles strong caustic and concentrated hydroxide splash; isophthalic polyester may cover a mild dilute alkaline rinse after the resistance record is reviewed, and epoxy is held for a notably aggressive or hotter solution. A general matrix is not specified where concentrated alkali pools at a stand.
- Depth and family: molded 38 mm fills the mixer stand and vessel walk cut around equipment; pultruded I-bar follows the floor runs. The coarser 50×50 opening sheds hydroxide and powder faster; span and walking duty set the depth.
- Film finish: grit-embedded top at the hose standing spots; concave dished members along the recovery trench shed damp film; smooth mesh kept for sheltered corners clear of drips.
- Worked example: a vinyl-ester molded 38 mm 50×50 over a 900 mm single clear span, checked to L/200, gives about 10 kN/m² for distributed walking only. The figure omits spill weight, vessel handling and trolley wheels; alkali compatibility follows the resistance chart, and the matched report sets the final span.
- Powder watch: crystalline buildup at edges or in openings concentrates alkali as it dries; rinse it before it bakes onto the face, and inspect any bar where efflorescence or swelling has begun.
3. Installation and Bearing Details
- Mark the mixer, vessels and recovery trench before seating panels; confirm the alkali sump takes rinse water away from the makeup stand.
- Rest sections on the isolation bedding over steel, keeping node end and side clearances around vessel plinths, pump bases and line unions.
- Hold each support and corner with the stainless clip suited to the section; snug by hand to the fitting setting, leaving hatch panels free to lift.
- Close sawn edges and drilled holes beside the plinth cut-outs with matched resin; after a release rinse, verify the panel drains and powder has not packed in the mesh.
- ≥ 50 mm bearing on steel/FRP support; 60 mm preferred at end spans
- 3 mm neoprene strip on steel supports to cut galvanic contact and local stress
- 10–15 mm end gap for thermal movement (~20 mm at long runs)
- 6–10 mm side gap for expansion and safe lifting
- Clips at every support and every corner; C/L/T/W/saddle families; A2-70 M6/M8 bolts
- Hand-tighten plus 1/4 turn; do not over-torque
- Seal any cut edge with matched resin within 24 hours
- Walk the deck and re-torque after 2 weeks of service
4. Routine Inspection and Maintenance
| Task | Frequency | What to check |
|---|---|---|
| Visual inspection | Monthly | Cracked bars, loose clips, edge seal, displaced panels |
| Clip torque check | Quarterly, first year | Hand-tight; re-torque any loose fixing |
| Washdown | As needed | Fresh water, low pressure; no acid or solvent-based cleaner |
| Grit top renewal | As needed | Top up worn traction with matched gritted resin |
| Edge seal check | Annually | Touch up any bare roving before it spreads |
| UV top-coat | Every 3–5 years | Re-coat exposed surface with matched resin on request |
- Inspect mixer stands and vessel edges for swelling, dull efflorescence, crazing or powdery residue holding alkali against the bar.
- Watch fixings and hatch panels near the mixer for vibration looseness, and check vessel-foot corners for cracking.
- Rinse alkali powder toward the sump with clean water at low pressure; keep solvent or an incompatible cleaner off the matrix.
- Renew worn grit and bare fibre at edges; log panels with matrix swelling for resin-grade review rather than a surface coat.
5. RFQ Inputs and Procurement Checklist
- Record the alkali present: product, concentration, temperature, neat splash versus diluted washdown.
- Give plant layout, mixer and vessel positions, floor span, sump trench route and the duty pattern: connection visits, line carry or occasional trolley.
- Mark mixer stands, damp floor stretches and sheltered corners with the finish wanted in each.
- Attach the platform drawing showing vessels, pumps, drain lines, sump, plinths and hatch panels.
- Reference the governing standard and deflection limit; request the matched resistance note, batch record and hardness check, and confirm vessel or trolley handling through factory engineering.
- Governing access standard and project deflection limit are cited with the order.
- Matched resistance note confirms the resin grade against the recorded medium.
- Batch material record and Barcol hardness check accompany the delivered panels.
- Any point, wheel, concentrated or equipment load is referred to engineer review and the matched report.
| Minimum order (MOQ) | 10 m² |
| Standard production | 15–25 working days after drawing approval |
| Overall lead time | 12–36 working days overall |
| Indicative price | USD 15–95/m² |
| Manufacturing history | Founded 2004; 200+ employees; 20,000+ m² plant |
| Export reach | 45+ countries; 541+ customer reviews, 4.9/5 average rating |
6. Compliance and Service Boundaries
7. Frequently Asked Questions
Which matrix resists caustic and hydroxide splash?
Vinyl ester handles strong caustic and concentrated hydroxide; isophthalic polyester may cover a mild dilute rinse after review, with epoxy held for a more aggressive or hotter solution.
How does alkali attack a composite member?
Through swelling, dull efflorescence or crazing at a drip or edge; dried crystals concentrate hydroxide against the bar, so powder is rinsed before it builds on the face.
How should the caustic platform shed liquid?
The opening drains hydroxide and rinse water to the recovery sump; a coarse 50×50 mesh sheds powder faster, and panels are checked so crystals do not pack the openings.
Does the deck carry the vessels or pumps?
No. Vessels, pumps and their loads rest on the plinth or frame; the walking and spill-catching surface only. Vessel and trolley loads need engineer review.
Which alkali details belong on the enquiry?
Product, concentration, temperature, neat versus diluted contact, plus sump trench and spill-tray positions; these set the grade against the resistance chart.