Check the recorded acetone against the resistance reference before selecting any resin, choose a cleaning-station traction finish, seal every cut edge, isolate fixings, and supply composition, exposure and duty in the RFQ; ketone service proceeds only on a compatible documented basis.
- Ketone tolerance is checked family by family; where acetone sits outside a resin's scope, that family is not specified for the cleaning duty, and a compatible system or documented test is sought instead.
- Molded 38 mm suits cleaning bays and storage surrounds cut around parts and drains; pultruded sections follow longer channel runs. Span, parts access.
- Grit top for pads where feet stay damp or slippery; concave dished sections shed films on ledges, and smooth mesh stays off the wipe-down splash line. Every cut and hole closes with matched resin; an open edge lets ketone reach the glass and undercut the laminate from the cut side.
How this article differs: This page covers the ketone cleaning duty and procurement inputs; it does not re-derive load tables, concentrated-load checks or resin chemistry, which are handled in the dedicated reference articles.
1. Site Conditions and Duty
Acetone is a fast-evaporating ketone used for equipment and part cleaning, coating thinning, adhesive prep and general degreasing. Grating in the cleaning station, parts-wash area and solvent storage point meets wipe-down splash, thin films left on bars after a spill, vapour that settles in low corners, and runoff toward the drain. The area is intermittently wet rather than continuously immersed; because acetone evaporates quickly, residue may be light but the repeated thin-film contact across shifts still bears on the resin surface.
Ketones are among the more demanding solvents for thermoset resins: they soften, swell or attack certain polyester and vinyl ester matrices even at room temperature, and some resin families are explicitly not recommended for ketone contact. The recorded acetone purity and any blended thinner matter; compatibility follows the resistance tables, and where the resin is marginal the deck should not be specified from a general solvent label. An unsealed cut or fixing hole gives ketone vapour and liquid a direct path into the laminate, so edge condition and clip isolation are critical.
2. Build-up, Resin and Surface Selection
| Location | Exposure mode | Duty | Suggested build-up | Resin / surface note |
|---|---|---|---|---|
| Parts cleaning station | Wipe-down splash, thin film, vapour | Rounds during cleaning cycles | Molded 38 mm 38×38 | Resin checked vs ketone; grit top |
| Solvent storage point | Leak film, drum runoff | Walking and container handling | Molded 38 mm 50×50 | Matched family; concave shed |
| Wash / drain cover | Intermittent runoff, pooled rinse | Cover over collection channel | Pultruded 38 mm T-bar | Sealed edge; impervious finish |
| Decanting ledge | Drips and wipe-down | Standing reach on transfer | Molded 38 mm cut-to-size | Grip finish where damp |
- Ketone tolerance is checked family by family; where acetone sits outside a resin's scope, that family is not specified for the cleaning duty, and a compatible system or documented test is sought instead.
- Molded 38 mm suits cleaning bays and storage surrounds cut around parts and drains; pultruded sections follow longer channel runs. Span, parts access.
- Grit top for pads where feet stay damp or slippery; concave dished sections shed films on ledges, and smooth mesh stays off the wipe-down splash line. Every cut and hole closes with matched resin; an open edge lets ketone reach the glass and undercut the laminate from the cut side.
3. Installation and Bearing Details
- Level the station bearers and drain ledges, clearing solvent film before dry-fitting; an uneven seat traps residue at panel edges.
- Bed sections on the 3 mm neoprene isolation strip over steel, retaining end and side gaps from the node detail around parts racks and valves.
- Fix with the matching clip family at every bearer and corner; isolate the fastener from dissimilar metal and hand-tighten to setting rather than over-driving.
- Seal cut edges and drilled holes within 24 hours; lift drain covers without prising neighbours, then re-check bearing and clips after the first two weeks of ketone service.
- ≥ 50 mm bearing on steel/FRP support; 60 mm preferred at end spans
- 3 mm neoprene strip on steel supports to cut galvanic contact and local stress
- 10–15 mm end gap for thermal movement (~20 mm at long runs)
- 6–10 mm side gap for expansion and safe lifting
- Clips at every support and every corner; C/L/T/W/saddle families; A2-70 M6/M8 bolts
- Hand-tighten plus 1/4 turn; do not over-torque
- Seal any cut edge with matched resin within 24 hours
- Walk the deck and re-torque after 2 weeks of service
4. Routine Inspection and Maintenance
| Task | Frequency | What to check |
|---|---|---|
| Visual inspection | Monthly | Cracked bars, loose clips, edge seal, displaced panels |
| Clip torque check | Quarterly, first year | Hand-tight; re-torque any loose fixing |
| Washdown | As needed | Fresh water, low pressure; no acid or solvent-based cleaner |
| Grit top renewal | As needed | Top up worn traction with matched gritted resin |
| Edge seal check | Annually | Touch up any bare roving before it spreads |
| UV top-coat | Every 3–5 years | Re-coat exposed surface with matched resin on request |
- Walk the station and storage point monthly for tacky or softened bars, loose clips, shifted covers and film in low corners.
- Check clip torque quarterly in year one; free any seized fitting before it locks under solvent residue.
- Clean per the site ketone-handling procedure; avoid repeated ketone wiping and abrasive scrubbing on the matrix.
- Renew worn grit with matched gritted resin and touch up exposed roving at edges before swelling spreads.
5. RFQ Inputs and Procurement Checklist
- State the acetone purity and any blended thinner, plus recorded ambient or operating temperature.
- Describe exposure: vapour only, wipe-down film on bars, intermittent splash, or pooled liquid in the sump, and contact frequency through the shift.
- Give the duty: cleaning rounds, parts handling, decanting or equipment reach, and any local load from containers or tools.
- Mark finishes by zone: grit on damp or slippery pads, concave on ledges, smooth on dry sheltered points.
- Cite the governing standard and deflection limit; request the matched resistance check, batch material record and Barcol hardness with the order papers.
- Governing access standard and project deflection limit are cited with the order.
- Matched resistance note confirms the resin grade against the recorded medium.
- Batch material record and Barcol hardness check accompany the delivered panels.
- Any point, wheel, concentrated or equipment load is referred to engineer review and the matched report.
| Minimum order (MOQ) | 10 m² |
| Standard production | 15–25 working days after drawing approval |
| Overall lead time | 12–36 working days overall |
| Indicative price | USD 15–95/m² |
| Manufacturing history | Founded 2004; 200+ employees; 20,000+ m² plant |
| Export reach | 45+ countries; 541+ customer reviews, 4.9/5 average rating |
6. Compliance and Service Boundaries
7. Frequently Asked Questions
Which resin tolerates acetone and ketones on grating?
Ketone tolerance is checked family by family against the resistance reference; some polyester and vinyl ester systems are not recommended for ketone contact. Where acetone sits outside a family's scope, do not specify it for the duty; seek a compatible system or documented test.
Molded or pultruded in a parts cleaning station?
Molded 38 mm suits cleaning bays and storage surrounds cut around parts and drains; pultruded sections follow longer channel runs. The measured span, parts access and fittings decide the mix.
What finish handles a damp ketone area?
Grit-embedded top for pads where feet stay damp or slippery; concave dished sections shed films on ledges; keep smooth panels off the wipe-down line. Match the opening to site footwear.
How are cut edges and fixings protected from ketone?
Every cut and hole is sealed with matched resin within 24 hours; sections bed on the neoprene strip and matching clips isolate fasteners from dissimilar metal. Clearances follow the node drawing.
What ketone damage signals require review?
Softened or tacky skin, swelling, blushing, dulling, persistent odour on bars, loose roving at edges or lifting seal should be flagged for engineering review; do not reuse a panel whose laminate has swollen or opened to the glass.